Hot rolled plate & coil

Boiler & pressure vessel steel plate

Boiler & pressure vessel steel plate for boilers, pressure vessels and process equipment made to the specified design code. Select the grade, dimensions, finish and inspection requirements for your order.

Product form
Plate
Surface / finish
Hot rolled / heat treated
Grade / standard
ASTM A516, A285, A387, A515, A537 and additional specifications

Product details

Boiler & pressure vessel steel plate for boilers, pressure vessels and process equipment made to the specified design code. Select the grade, dimensions, finish and inspection requirements for your order.

Grade selection

Select the exact grade and purchasing standard from the tables below.

Delivery condition

Specify surface finish, heat treatment and dimensional tolerances.

Inspection & supply

Agree test documentation, packing and shipment requirements.

Typical application

Boilers, pressure vessels and process equipment made to the specified design code.

Boilers, pressure vessels and process equipment made to the specified design code.

Explore applications

Product specifications

Product specifications for Boiler & pressure vessel steel plate
Product formPlate
Grade / standardASTM A516, A285, A387, A515, A537 and additional specifications
Width100–3,000 mm reference supply range
Manufacturing processHot rolled; final heat treatment according to the selected grade
Cut length1–12 m or cut to order
Delivery conditionAs rolled, normalized or quenched and tempered only as permitted by the selected grade
ThicknessTo the selected grade and plate specification
Dimensional tolerancesTo the ordered product standard and agreed drawing
InspectionMaterial identification, dimensions, surface and specified test report
PackagingProtective wrapping, edge protection and steel strapping as agreed

Ranges vary with grade, finish and order specification. Confirm the required dimensions, coating and availability in your quotation.

Grade-specific technical data

Select a grade to view its composition, mechanical properties and applicable test conditions.

A202

A202 — chemical composition (%)

A202Chemical Element Content(Upper Limit%)
CSiMnPSCr
GradeA0.170.54-0.960.97-1.520.0350.0350.31-0.64
GradeB0.250.54-0.960.97-1.520.0350.0350.31-0.64

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A202Tensile Strengthksi [MPa]Yield Strength ksi [MPa]Elongation Gauge length 8in.[200mm],%Elongation Gauge length 2in.[50mm],%
GradeA75-95 [515-655]45 [310]≧ 16≧ 19
GradeB85-110 [585-760]47 [325]≧ 15≧ 18

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A202 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

A203

A203 — chemical composition (%)

A203  Upper limit of Chemical Element Content(%)
CSiMnPSNi
Class A0.230.13-0.450.880.0250.0252.03-2.57
Class B0.250.13-0.450.880.0250.0252.03-2.57
Class D0.200.13-0.450.880.0250.0253.18-3.82
Class E0.230.13-0.450.880.0250.0253.18-3.82
Class F0.230.13-0.450.880.0250.0253.18-3.82

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A202Tensile Strengthksi [MPa]Yield Strength ksi [MPa]Elongation Gauge length 8in.[200mm],%Elongation Gauge length 2in.[50mm],%
GradeA65-85 [450-585]37 [255]1923
GradeB70-90 [485-620]40 [275]1721
GradeD65-85 [450-585]37 [255]1923
GradeE70-90 [485-620]40 [275]1721
GradeF75-100 [515-690]50 [345]-20

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A203 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

A204

A204 — chemical composition (%)

A204Upper limit of Chemical Element Content (%)
CSiMnPSMo
Class A0.18-0.250.13-0.450.90-0.980.0350.0350.45-0.60
Class B0.20-0.270.13-0.450.90-0.980.0350.0350.45-0.60
Class C0.23-0.280.13-0.450.90-0.980.0350.0350.45-0.60

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A204Tensile Strength ksi [MPa]Yield Strength ksi [MPa]Elongation Gauge length 8in.[200mm],%Elongation Gauge length 2in.[50mm],%
GradeA70-90 [485-620]37 [255]1923
GradeB75-95 [515-655]40 [275]1721
GradeC75-95 [515-655]43 [295]1620

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A204 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

A285

A285 — chemical composition (%)

A285CMnPS
Class A0.170.980.0250.025
Class B0.220.980.0250.025
Class C0.280.980.0250.025

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A285Thickness mmYield MpaTensile Strength MpaElongation(%)
Class A6-50165310-45030%
50-200165310-45027%
Class B6-50185345-48528%
50-200185345-48525%
Class C6-50205380-51527%
50-200205380-51523%

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A285 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

A387

A387 — chemical composition (%)

A387UNSCMnPSSiCrMo
Level 5S50200≤ 0.150.25-0.660.0250.025≤ 0.553.90-6.100.40-0.70
Level 9K90941≤ 0.150.25-0.660.0250.025≤ 1.057.90-10.100.85-1.15
Level 11K117890.04-0.170.35-0.730.0250.0250.44-0.860.94-1.560.40-0.70
Level 12K117570.04-0.170.35-0.730.0250.0250.13-0.450.74-1.210.40-0.65
Level 22K215900.04-0.150.25-0.660.0250.025≤ 0.501.88-2.620.85-1.15
Class 22LK21590≤ 0.120.25-0.660.0250.025≤ 0.501.88-2.620.85-1.15
Class 91K909010.06-0.150.25-0.660.0250.0120.18-0.567.90-9.600.80-1.10

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A387CategoryTensile Strength MpaYield Strength MpaElongation Gauge length 2in.[50mm]%
Level 5  Section Category 1415-58520518
Section Category 2515-69031018
Level 9  Section Category 1415-58520518
Section Category 2515-69031018
Level 11  Section Category 1415-58524022
Section Category 2485-62031022
Level 12  Section Category 1380-55023022
Section Category 2450-58527522
Level 22  Section Category 1415-58520518
Section Category 2515-69031018

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A387 — physical properties

PropertyMetric
Density7.7–8.03 g/cm³

Typical range varies with chromium–molybdenum grade. The source’s duplicate metric value under its imperial heading is omitted.

A516

A516 — chemical composition (%)

A516C Thickness (mm)Mn Thickness (mm)SiPS
6-12.5mm12.5-25mm25-50mm>50mm≤ 12.5mm>12.5mm
Level 550.180.200.220.250.55~0.980.60~1.300.13~0.450.0350.035
Level 600.210.230.230.250.6~0.90.80~1.200.13~0.450.0350.035
Level 650.240.260.260.280.85~1.200.85~1.200.13~0.450.0350.035
Level 700.270.280.280.30.85~1.200.85~1.200.13~0.450.0350.035

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

ASTM A516  Tensile StrengthYieldLower limit of Elongation(%)
(MPa)(MPa)Gauge Length 50mmGauge Length 200mm
Level 55380~5152052723
Level 60415~5502202521
Level 65450~5852402319
Level 70485~6202602117

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A516 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

A533

A533 — chemical composition (%)

A533 Class AClass BClass CClass DClass E
C 0.250.250.250.250.20
MnSmelting Analysis1.15-1.501.15-1.501.15-1.501.15-1.501.15-1.70
Finished Product Analysis1.07-1.621.07-1.621.07-1.621.07-1.621.04-1.84
P 0.0250.0250.0250.0250.020
S 0.0250.0250.0250.0250.015
SiSmelting Analysis0.15-0.400.15-0.400.15-0.400.15-0.400.15-0.40
Finished Product Analysis0.13-0.450.13-0.450.13-0.450.13-0.450.13-0.45
MoSmelting Analysis0.45-0.600.45-0.600.45-0.600.45-0.600.25-0.60
Finished Product Analysis0.41-0.640.41-0.640.41-0.640.41-0.640.21-0.64
NiSmelting Analysis-0.40-0.700.70-1.000.20-0.400.60-1.00
Finished Product Analysis-0.37-0.730.67-1.030.17-0.430.57-1.03
CrSmelting Analysis----0.60
Finished Product Analysis----0.64

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A533Tensile Strength Ksi(MPa)Yield Strength Ksi(MPa)Elongation Gauge Length 2in.[50mm],%
Grade180-100[550-690]50[345]18
Grade290-115[620-795]70[485]16
Grade3100-125[690-860]83[570]16

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A533 — physical properties

Physical PerformanceMetricImperial
Density7.7-8.03 g/cm30.278-0.290 lb/in3

Typical reference density, not a guaranteed mechanical acceptance value.

A537

A537 — chemical composition (%)

StandardThickness(Mm)CSiMnPSCuNiCrMo
A537≤ 40mm0.240.15-0.500.70-1.350.0350.0350.350.250.250.08
>40mm1.00-1.60

Grade-specific supplier reference. Preserve the stated thickness and heat/product-analysis basis; ranges are not interchangeable with a single maximum. Confirm the ordered standard edition and material certificate.

Mechanical properties — supplier grade table

A537Thickness mmYield MpaTensile Strength MpaElongation %
Level 1≤ 65345485-62022
65-100310450-585-
100-150--18
Level 2≤ 65415550-69022
65-100380515-65520
100-150315485-620-
Level 3≤ 65380550-69022
66-100345515-65520
101-150275485-620-

Product-matched supplier reference. Heat treatment, thickness and test orientation must match the purchase specification.

A537 — physical properties

Physical PerformanceMetricImperial
Density7.80g/cc0.282 lb/in³

Typical reference density, not a guaranteed mechanical acceptance value.

ASTM A515 grades 60 / 65 / 70

A515 — carbon maximum by plate thickness

Thickness (mm)Grade 60 / 415 C max. %Grade 65 / 450 C max. %Grade 70 / 485 C max. %
≤25.24.28.31
>25–50.27.31.33
>50–100.29.33.35
>100–200.31.33.35
>200.31.33.35

ASTM A515/A515M-17 (2022); heat and product analysis.

A515 — remaining chemical requirements

Element / analysisGrade 60Grade 65Grade 70
Mn max., heat0.900.901.20
Mn max., product0.980.981.30
P max.0.0250.0250.025
S max.0.0250.0250.025
Si, heat0.15–0.400.15–0.400.15–0.40
Si, product0.13–0.450.13–0.450.13–0.45

Mass %. For each 0.01 percentage-point carbon reduction below maximum, Mn may increase by 0.06, up to 1.50% heat / 1.60% product analysis. These limits use the 2022 reaffirmed edition, not older supplier tables.

A515 — tensile requirements

GradeYield min. (MPa)Tensile (MPa)A200 min. (%)A50 min. (%)
60 / 415220415–5502125
65 / 450240450–5851923
70 / 485260485–6201721

Elongation adjustments follow ASTM A20/A20M.

A515 — heat treatment and inspection

ParameterRequirement
Thickness ≤50 mmNormally as rolled; normalized and/or stress relieved when ordered
Thickness >50 mmNormalized
SteelmakingKilled steel, coarse austenitic grain practice
General plate requirementsASTM A20/A20M
Coil-derived plateQualification applies only after processing into finished plate and the required tests
Ultrasonic examinationASTM A435 / A577 / A578 when the applicable supplementary requirement is ordered

A515 is for intermediate/higher-temperature pressure-vessel plate. Do not assign a universal low-temperature impact guarantee.

Surface & processing requirements

Include the downstream process in your enquiry so that the material, dimensions and surface can be reviewed together.

Cut-to-size requirementsFinal length and width, cutting method and edge condition.
Forming / fabricationDescribe the downstream forming, pressing, profiling or fabrication operation.
Finishing requirementsState whether material will be painted, coated or otherwise finished after delivery.
Plate / sheet handlingConfirm lifting method, stack height and protection of edges and surfaces.

Production & processing

Define the material and the downstream process together. Cutting, slitting or finishing requirements should form part of the order specification.

Material review

Grade, dimensions and surface requirements are checked against the enquiry.

Processing scope

Agree cutting, slitting or forming requirements and the finished product tolerances.

Order inspection

Define acceptance criteria, identification and the requested documentation.

Rolling, processing and production facilities
Rolling, processing and production facilities
Explore manufacturing

Stock & warehouse

Hot rolled, galvanized and color coated material in warehouse settings. Ask our team to confirm current availability for your grade, dimensions and quantity.

Plate and sheet stock in covered storage
Plate and sheet stock in covered storage

Quality inspection & documentation

Agree the acceptance criteria and required documents before confirming your order.

  • Material identificationGrade, standard and requested test documentation.
  • Dimensions & surfaceThickness, width, finish and agreed tolerances.
  • Order documentsProduct identification, packing list and inspection scope.
Quality requirements
Coordinate measuring equipment
Coordinate measuring equipment
Ultrasonic thickness measurement
Ultrasonic thickness measurement
Hardness testing
Hardness testing
Tensile testing equipment
Tensile testing equipment
Chemical analysis laboratory
Chemical analysis laboratory
Metallographic examination
Metallographic examination

Packaging & shipment

Tell us how the material will be transported, unloaded and stored. Specify moisture protection, edge protection, package weight and destination with your enquiry.

Protective packing, loading and export shipment
Protective packing, loading and export shipment
ProtectionMoisture barrier, edge protection and surface protection as agreed.
Unit weightSpecify the coil or bundle weight for your unloading equipment.
IdentificationProduct, grade, dimensions and order reference on the agreed packing list.
DeliveryConfirm destination, transport method and delivery terms in the quotation.

Certificates & verification documents

Request the original document issued for the supplying company, product scope and order. Material test reports and conformity documents are checked against the named holder, issuing body and validity period.

Material test reportHeat or coil number, ordered grade, chemical composition and mechanical test results.
Inspection documentSpecify the required EN 10204 document type and inspection scope in the enquiry.
Conformity documentsRequest an original copy showing the issuing body, holder, number, applicable scope and validity.
Request applicable documents

Frequently asked questions

What should I include in my enquiry?

Send the product, grade or standard, dimensions, quantity, required finish and destination. Describe the end use if the specification is still being developed.

Can I request a particular size or finish?

Yes, include your required size and finish in the enquiry. Availability and any processing requirements must be confirmed in the quotation.

How are minimum order and lead time confirmed?

They depend on grade, dimensions, processing and quantity. We confirm them for the particular order rather than publish one figure for every product.

What documents should I request?

State the material test document, inspection scope and other purchasing documents required for your project. Agree these with the order.

Contact QR codeRequest a quote